煤矸石粉煤灰頁巖燒結磚的研制
發布時間: 2006-04-02 00:00 查看: 3754次
付勇堅 肖秋國 劉小波
以工業廢渣煤矸石、粉煤灰及風化頁巖為主要原料研制成燒結磚,具有較明顯的社會效益和經濟效益。介紹了原料的性能、配方組成、工藝、產品性能;指出選用粘結劑,采用高壓真空擠出成型工藝可提高半成品干燥強度;燒成升溫速度在300 ℃以前以50~80 ℃/h,300 ℃以后以100 ℃/h左右為宜。
關鍵詞:煤矸石 粉煤灰 風化頁巖 燒結磚
Abstract:The developed sintered brick made from gangue and fly ash as industrial wastes as well as weathered shale as main raw materials has obviously social and economic benefits. This paper introduces performance of raw materials, formula composition, production process and product performance. It points out that the high pressure vacuum extruded forming process with selected glue can increase the dry strength of semi-product. The sintering temperature boostings of 50~80 ℃/h before 300 ℃ and 100 ℃/h after 300 ℃ are proper.
Keywords:gangue, fly ash, weathered shale, sintered brick
以工業廢渣煤矸石、粉煤灰及風化頁巖為主要原料研制成燒結磚,具有較明顯的社會效益和經濟效益。介紹了原料的性能、配方組成、工藝、產品性能;指出選用粘結劑,采用高壓真空擠出成型工藝可提高半成品干燥強度;燒成升溫速度在300 ℃以前以50~80 ℃/h,300 ℃以后以100 ℃/h左右為宜。
關鍵詞:煤矸石 粉煤灰 風化頁巖 燒結磚
Abstract:The developed sintered brick made from gangue and fly ash as industrial wastes as well as weathered shale as main raw materials has obviously social and economic benefits. This paper introduces performance of raw materials, formula composition, production process and product performance. It points out that the high pressure vacuum extruded forming process with selected glue can increase the dry strength of semi-product. The sintering temperature boostings of 50~80 ℃/h before 300 ℃ and 100 ℃/h after 300 ℃ are proper.
Keywords:gangue, fly ash, weathered shale, sintered brick
>> 相關內容
- 低品質粉煤灰的活性激發研究 (點擊:14927 次)
- 廢石膏粉煤灰石灰結合料的研究 (點擊:14987 次)
- 粉煤灰和礦渣影響混凝土碳化的因素及建議 (點擊:16363 次)
- 粉煤灰、礦粉復合雙摻在大體積混凝土配合比中的應用 (點擊:20505 次)
- 劣質粉煤灰對混凝土性能的影響探討 (點擊:20827 次)
- 【技術交流】煤矸石材料填筑路基施工研究 (點擊:15478 次)
- 粉煤灰水熱合成沸石分子篩的研究進展 (點擊:24124 次)
- 煤矸石特性與資源化利用研究分析,綜合利用依然是大難... (點擊:24355 次)
- 燃煤灰渣作為混凝土摻合料的新變化及其影響(原創) (點擊:24762 次)
#
最新技術資訊
更多>>